Composition Limits, Per Cent—Iron and Normal Impurities Constitute Remainder
ASTM/AISI
Grade
UNS
Number
C
Mn
P
Max.
S
Max.
Si
Cr
Mo
Pb
41L42
G41420
.40/.45
.75/1.00
.035
.040
.15/.35
.80/1.10
.15/.25
.15/.35
MECHANICAL PROPERTIES:
ASTM/AISI
Grade
Mechanical Properties
Tensile
Strenght
(ksi)
Yield
Strength
(ksi)
Elongation
in 2"
%
Reduction
of Area
%
4142
105/102
85/95
15/25
45/55
Condition of Steel
Typical Hardness
Average
Machinability
% of CD 1215
Brinell
Rockwell
Annealed Cold Drawn
215/235
B96/100
65
1 Ksi = 1000 psi With the addition of 0.15%–0.35% lead, machinability is increased approximately 25%, longitudinal mechanical properties are not appreciably affected.
Size in
Inches
Lbs.
Per Ft.
Est. Lbs.
12' Bar
5/16
.2875
3.450
3/8
.4141
4.969
7/16
.5636
6.763
1/2
.7361
8.833
9/16
.9316
11.18
5/8
1.150
13.80
11/16
1.392
16.70
3/4
1.656
19.87
7/8
2.254
27.05
15/16
2.588
31.06
Size in
Inches
Lbs.
Per Ft.
Est. Lbs.
12' Bar
1"
2.944
35.33
1-1/8
3.727
44.72
1-1/4
4.601
55.21
1-5/16
5.072
60.86
1-1/2
6.625
79.50
1-5/8
7.775
93.30
2"
11.78
141.4
2-1/4
14.91
178.9
3"
26.50
318.0
”H” Band version available
Disclaimer: All technical data throughout this site is given only as an indication of what may be expected and should under no circumstances be used in specifying the raw materials. The technical data throughout this site has been obtained from a variety of sources we believe to be accurate, but is NOT GUARANTEED. A & C Metals - Sawing, Inc. assumes no liability whatsoever for the use of or reliance upon this information.